  • Irradiation-crosslinked Low Smoke Zero Halogen (LSZH) flame retardant polyolefin cable material

Irradiation-crosslinked Low Smoke Zero Halogen (LSZH) flame retardant polyolefin cable material  is a polyolefin-based pellet material which is produced by mixing, plasticizing and granulating with accessory ingredients such as special modifiers, non-toxic and non-halogen flame retardants, antioxidants and lubricants.

1、Model, name and application of products

Model

grade

name 

application

WDZ-YJ-J105

Rad-J105

Irradiation-crosslinked Low Smoke Zero Halogen (LSZH) flame retardant polyolefin insulation material at 105

Electrical equipment used wire, automotive wire, electrical motor, UL standard wires and instrumentation lines;Materials comply with EU RoHS directive

WDZ-YJ-J125

Rad-J125

Irradiation-crosslinked Low Smoke Zero Halogen (LSZH) flame retardant polyolefin insulation material at 125

2、Executive Standard

GB/T 32129-2015

3products properties

The properties of products are shown in Table 1.

4、Processing

general extruder is used in processing with the aspect ratio of Low compression ratio screw L/D≥20. A low compression ratio screw is recommended in order to benefit the extrusion of highly filled halogen flame retardant cable materials. The recommended reference processing temperature is shown below:

 sections 

Section 1

Section 2

Section 3

Section 4  

Extruder head

die

temperature / 

130140

140145

145150

150155

145155

145155

5、Packaging, transportation and storage

PackagingNet weight per bag25±0.2kg. The inner bag is aluminum plastic composites and the outer bag is polypropylene woven/polyethylene/craft paper composites.

Transportation and storageNo exposure to sunshine and rain during transportation. It should be stored in clean, cool, dry and ventilated warehouse.

Table 1: Products properties sheet

Test item

Rad-J105

Rad-J125

Tensile strength/MPa ≥

10.0

10.0

Breaking elongation /% ≥

150

150

Air oven heat aging

135±2)℃×168 h

158±2)℃×168 h

change rate of Tensile strength /% ≤

±25

±25

change rate of Breaking elongation /% ≤

±25

±25

Impact brittle temperature

Test temperature/ 

-25

-25

Impact brittle property/number of failure

15/30

15/30

Thermal elongation

Test condition

200±3)℃×0.2 MPa×15min

elongation under load/% ≤

100

100

Permanent deformation after cooling /% ≤

25

25

volume resistivity  at 20 /Ω·m ≥

1.0×1012

1.0×1012

volume resistivity at working temperature

Test temperatur/ 

105±2

125±2

volume resistivity /Ω·m ≥

2.0×108

2.0×108

dielectric strength /MV/m 

20

20

oxygen index /% ≥

28

28

smoke density

flameless

350

350

flame

100

100

Acidity of combustion gas release

Content of HCL and HBr/% ≤

0.5

0.5

HF content /% ≤

0.1

0.1

pH 

4.3

4.3

electrical conductivity /μs/mm  

10

10

toxic hazards of  material-produced tobacco

Negotiating by supply and demand sides according to product applications demand.